      请问Cr12或者Cr12MoV属于不锈钢吗?

      [复制链接]
      发表于 2006-6-27 18:36:00 | 显示全部楼层
      <p>不锈钢还不一样会生锈!!</p><p>他只不过是里面c的含量低而已!</p>
      发表于 2006-7-2 04:18:00 | 显示全部楼层
      <p class="MsoNormal" style="MARGIN: 0cm 0cm 0pt;"><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">不锈钢之所以具有不锈性,关键是由于钢中含有铬。所需要的最低铬含量美国、欧洲标准中规定为不小于</span><span lang="EN-US"><font face="Times New Roman">10.5%</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">,日本工业标准规定一般不小于约</span><span lang="EN-US"><font face="Times New Roman">11%</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">,我国一般认为不小于</span><span lang="EN-US"><font face="Times New Roman">12%</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">。</span></p><p class="MsoNormal" style="MARGIN: 0cm 0cm 0pt;"><span lang="EN-US"><font face="Times New Roman">C</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">易锈,所以不锈钢低碳,大部分</span><span lang="EN-US"><font face="Times New Roman">0.1%</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">级别,少部分马氏体不锈钢</span><span lang="EN-US"><font face="Times New Roman">1%C</font></span><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">。</span></p><p class="MsoNormal" style="MARGIN: 0cm 0cm 0pt;"><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">冷作模具钢要高碳高铬以提高淬透性。</span></p><p class="MsoNormal" style="MARGIN: 0cm 0cm 0pt;"><span style="FONT-FAMILY: 宋体; mso-ascii-font-family: &quot;Times New Roman&quot;; mso-hansi-font-family: &quot;Times New Roman&quot;;">磁性弱一般认为有过冷奥氏体。</span></p><p class="MsoNormal" style="MARGIN: 0cm 0cm 0pt;"><span style="COLOR: black; FONT-FAMILY: 宋体; mso-ascii-font-family: Tahoma; mso-hansi-font-family: Tahoma; mso-bidi-font-size: 9.0pt; mso-bidi-font-family: Tahoma;">楼主提供的成分显然是</span><span lang="EN-US" style="COLOR: black; FONT-FAMILY: Tahoma; mso-bidi-font-size: 9.0pt;">Cr12</span><span style="COLOR: black; FONT-FAMILY: 宋体; mso-ascii-font-family: Tahoma; mso-hansi-font-family: Tahoma; mso-bidi-font-size: 9.0pt; mso-bidi-font-family: Tahoma;">,很难能达</span><span lang="EN-US" style="COLOR: black; FONT-FAMILY: Tahoma; mso-bidi-font-size: 9.0pt;">HRC64</span><span style="COLOR: black; FONT-FAMILY: 宋体; mso-ascii-font-family: Tahoma; mso-hansi-font-family: Tahoma; mso-bidi-font-size: 9.0pt; mso-bidi-font-family: Tahoma;">,这种硬度是高速钢的水平了。</span><span lang="EN-US" style="COLOR: black; FONT-FAMILY: Tahoma; mso-bidi-font-size: 9.0pt;"><p></p></span></p><span lang="EN-US" style="FONT-SIZE: 10.5pt; COLOR: black; FONT-FAMILY: Tahoma; mso-bidi-font-size: 9.0pt; mso-fareast-font-family: 宋体; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA;">Cr12MoV</span><span style="FONT-SIZE: 10.5pt; COLOR: black; FONT-FAMILY: 宋体; mso-ascii-font-family: Tahoma; mso-hansi-font-family: Tahoma; mso-bidi-font-size: 9.0pt; mso-bidi-font-family: Tahoma; mso-font-kerning: 1.0pt; mso-ansi-language: EN-US; mso-fareast-language: ZH-CN; mso-bidi-language: AR-SA;">的碳也超标了,不能算不锈钢。</span>
      发表于 2006-7-4 07:54:00 | 显示全部楼层
      Cr12或者Cr12MoV属于高铬模具钢
      发表于 2006-7-5 17:47:00 | 显示全部楼层
      <p>怪不得找不到好工作!</p><p>几本书都没读好!更不敢谈什么林林总总的实践!</p><p>当然不是全盘否定,</p><p>看一下论坛上绝大多数帖子水平实在不怎么样!太多让人甚至伤心!</p>
      发表于 2006-7-8 21:32:00 | 显示全部楼层
      Cr后面跟大于12的为不锈钢淬火后HRC58-62
      发表于 2006-7-10 17:34:00 | 显示全部楼层
      我觉得cr12应该是合金工具钢.不会是不锈钢!
      发表于 2006-7-15 11:57:00 | 显示全部楼层
      铬含量超过13%才不会生锈,这时候铬会与空气形成致密氧化层,起抗氧化作用
      发表于 2006-9-21 19:01:00 | 显示全部楼层
      cr12真的很硬
      发表于 2006-9-23 07:54:00 | 显示全部楼层
      <p>不是不锈钢</p>
      发表于 2006-9-24 15:32:00 | 显示全部楼层
      附一份世界各国不锈钢标准钢号对照表给你查查<br/>
      [此贴子已经被作者于2006-9-24 15:36:01编辑过]

      发表于 2006-9-24 22:38:00 | 显示全部楼层
      NO\NO\是冷作钢
      发表于 2007-1-11 15:21:00 | 显示全部楼层
      <p>好像是模具刚钢....</p>
      [此贴子已经被作者于2007-1-11 15:21:30编辑过]

      发表于 2007-1-21 15:53:00 | 显示全部楼层
      [em40]就牌号而言,应该不是
      发表于 2007-8-10 17:12:00 | 显示全部楼层
      他是模具材料,不修铁才受慈,不锈钢不受慈
      发表于 2007-8-23 20:18:00 | 显示全部楼层
      Cr12和Cr12MoV是合金工具钢,用于冲压模具。
      发表于 2007-8-24 21:49:00 | 显示全部楼层
      <p>Cr12,Cr12MoV,Cr4W2MoV属于高合金工具钢.</p>
      发表于 2007-8-24 21:56:00 | 显示全部楼层
      <p>用于制造冷作模具用.有高的淬透性,耐耐磨性,热处理变形小,由于碳化物分布不均匀而导致强度低.HRC58~60.</p>
      发表于 2007-8-25 09:22:00 | 显示全部楼层
      你是搞模具这一行的吗?
      发表于 2007-8-26 22:55:00 | 显示全部楼层
      <p>是不是搞错了,Cr12会是不锈钢吗?</p>
      发表于 2007-8-28 14:15:00 | 显示全部楼层
      Cr12、Cr12MoV是冷冲压模具钢材,内部组织属于莱氏体钢材,可以看一下:汽车模具---Cr12MoV焊接工艺的帖子。
      您需要登录后才可以回帖 登录 | 注册

      本版积分规则

      关闭

      招聘信息 上一条 /5 下一条

      关闭

      求职信息 上一条 /5 下一条

      关闭

      技术求助 上一条 /5 下一条

      QQ|小黑屋|手机版|模具论坛 ( 浙ICP备15037217号 )

      GMT+8, 2025-5-14 05:13

      Powered by Discuz! X3.4

      © 2001-2013 Comsenz Inc.

      快速回复
      返回顶部
      返回列表
       
      客服电话:0577-61318188
      模具论坛交流群:
      模具论坛交流群
      工作时间:
      08:30-17:30